FRACTOGRAPHIC LOGGING FOR DETERMINATION OF PRE-CORE AND CORE-INDUCED FRACTURES

NICHOLAS COMBS NO. 7239 WELL, HAZARD, KENTUCKY

Data and Resources

Additional Info

Field Value
Author Isabella Cross-Najafi
Last Updated August 8, 2019, 03:12 (EDT)
Created August 8, 2019, 03:12 (EDT)
Citation "\"BYRON R. KULANDER, STUART L. DEAN, AND CHRISTOPHER C. BARTON \""
Is NETL associated "\"No\""
Publication Date "\"01/01/1977\""
spatial "\"{\"type\":\"MultiPolygon\",\"coordinates\": [[[[-88.04276, 36.49657], [-89.53327, 36.49817], [-89.56706, 36.5188], [-89.56823, 36.54147], [-89.55621, 36.557804], [-89.169624, 37.064285], [-89.14642, 37.093235], [-89.0651, 37.185913], [-87.9219, 37.91991], [-84.742874, 39.142063], [-84.444916, 39.111828], [-82.89031, 38.742775], [-82.61375, 38.472668], [-81.95957, 37.531174], [-82.878044, 36.893696], [-83.13851, 36.74006], [-83.69561, 36.584248], [-88.04276, 36.49657]]]]}\""